Vestamid HTplus - PPA - Evonik Operations GmbH
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Vestamid HTplus" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
For weight and function optimization of a Lotus Exige racing car belonging to the RED motor racing team, a charge-air duct made from PPA (polyphthalamide; grade: Vestamid HTplus, manufacturer: Evonik Degussa GmbH) was developed within a few weeks and the existing aluminum pipe replaced (Fig. 1). The PPA charge-air duct proved successful in the 2008 season under the extreme conditions encountered in motor racing. The RED motor racing team achieved top positions in 24 h races, for example. The adv...
Kunststoffe international, 2010-03-17, A Permanent Bond
...est beams (Title photo) were manufactured and mechanically assessed. The primary objective was to cover the range of materials that would mainly be used. Alongside the widely used PA6-GF30, material types such as PA6-GF50, PPA-GF30 (grade: Vestamid HTplus M1033, manufacturer: Evonik Degussa GmbH), PPA-GF50 (grade: Vestamid HTplus M1035) as well as PP-LGF30 were tested. Due to its cost advantage polypropylene is seeing increasing interest from OEMs alongside the commonly used PA6, not least of al...
Kunststoffe international, 2011-08-24, Looking for the Right Polymer
...is an engineering polymer whereas LCP and PPA are high-performance polymers. Also within individual classes of polymer, there are differences. Thus, Evonik Industries, Marl, recently launched one of the newest generations of PPA under the brand name Vestamid HTplus. The company distinguishes between two grades: a PA6T/X offering increased heat resistance and a PA10T/X having particularly low water absorption. PA10T/X is moreover 50 % bio-based and is sourced in part from vegetable oil instead of...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.